Specifications
- Type
- aluminium electrolytic, prototype
- Standard
- STAS 7675-73
- Capacitance (Cn)
- 6 different values (see Variants)
- Capacitance, min
- 4.7–220 µF (see Variants)
- Capacitance, max
- 4.7–220 µF (see Variants)
- Tolerance
- −10…+100 %; −10…+50 % (special)
- Rated voltage (Un)
- 6.3–63 V (see Variants)
- Dissipation factor (tan δ)
- ≤ 0.3 (Un = 6.3 V), ≤ 0.25 (Un = 10…40 V), ≤ 0.2 (Un = 63 V), at 100 Hz, 20 °C
- Reliability (failure rate λ)
- ≤ 1·10⁻⁶/h
- Leakage current (If)
- ≤ 0.006·CnUn [µF·V] + 4 µA (CnUn ≤ 1000 µF·V); ≤ 0.01·CnUn [µF·V] + 1 (CnUn ≥ 1000 µF·V), at 20 °C
- Ripple current (I~)
- 25–220 mA (see Variants)
- Climatic category
- 25/070/21
- Temperature range
- −25…+75 °C
- Package
- cylindrical, axial leads
- Diameter (D)
- 8–12 mm (see Variants)
- Length (L)
- 18–39 mm (see Variants)
- Lead spacing
- 22.5–45 mm (see Variants)
- Lead diameter (d)
- 0.8 mm
- Lead length (l)
- 38–50 mm (see Variants)
Variants (18)
| Note | Compare | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| EP 52.48 (6.3 V) | 47 µF | 47 | 47 | 6.3 | 60 | 8 | 18 | 22.5 | 38 | 1978–1979 catalogue | |
| EP 52.50 (6.3 V) | 100 µF | 100 | 100 | 6.3 | 110 | 8 | 24 | 30 | 38 | 1978–1979 catalogue | |
| EP 52.53 (6.3 V) | 220 µF | 220 | 220 | 6.3 | 190 | 9.5 | 24 | 30 | 38 | 1978–1979 catalogue | |
| EP 52.49 (10 V) | 47 µF | 47 | 47 | 10 | 70 | 8 | 21 | 25 | 38 | 1978–1979 catalogue | |
| EP 52.52 (10 V) | 100 µF | 100 | 100 | 10 | 120 | 9.5 | 21 | 25 | 38 | 1978–1979 catalogue | |
| EP 52.57 (10 V) | 220 µF | 220 | 220 | 10 | 220 | 12 | 24 | 30 | 50 | 1978–1979 catalogue | |
| EP 52.48 (16 V) | 22 µF | 22 | 22 | 16 | 50 | 8 | 18 | 22.5 | 38 | 1978–1979 catalogue | |
| EP 52.50 (16 V) | 47 µF | 47 | 47 | 16 | 100 | 8 | 24 | 30 | 38 | 1978–1979 catalogue | |
| EP 52.53 (16 V) | 100 µF | 100 | 100 | 16 | 140 | 9.5 | 24 | 30 | 38 | 1978–1979 catalogue | |
| EP 52.49 (25 V) | 22 µF | 22 | 22 | 25 | 50 | 8 | 21 | 25 | 38 | 1978–1979 catalogue | |
| EP 52.53 (25 V) | 47 µF | 47 | 47 | 25 | 110 | 9.5 | 24 | 30 | 38 | 1978–1979 catalogue | |
| EP 52.55 | 100 µF | 100 | 100 | 25 | 160 | 9.5 | 39 | 45 | 50 | 1978–1979 catalogue | |
| EP 52.49 (40 V) | 10 µF | 10 | 10 | 40 | 25 | 8 | 21 | 25 | 38 | 1978–1979 catalogue | |
| EP 52.52 (40 V) | 22 µF | 22 | 22 | 40 | 70 | 9.5 | 21 | 25 | 38 | 1978–1979 catalogue | |
| EP 52.57 (40 V) | 47 µF | 47 | 47 | 40 | 120 | 12 | 24 | 30 | 50 | 1978–1979 catalogue | |
| EP 52.49 (63 V) | 4.7 µF | 4.7 | 4.7 | 63 | 30 | 8 | 21 | 25 | 38 | 1978–1979 catalogue | |
| EP 52.52 (63 V) | 10 µF | 10 | 10 | 63 | 50 | 9.5 | 21 | 25 | 38 | 1978–1979 catalogue | |
| EP 52.57 (63 V) | 22 µF | 22 | 22 | 63 | 90 | 12 | 24 | 30 | 50 | 1978–1979 catalogue |
Click a column heading to sort. „+” adds a variant to the comparison (EP 5200).
Description
The EP 5200 is a prototype aluminium electrolytic capacitor of IPRS Băneasa, developed with the ET 5200 to extend service life and the rated temperature range [1]. IPRS made seven types of electrolytic capacitors, from 1 µF to 10,000 µF and from 3 V to 450 V [1].
The I.P.R.S. Băneasa Capacitors catalogue (1978–1979) lists the EP 52.00 among its electrolytic capacitors, as „Polarized miniature axial terminal electrolytic capacitors” („Condensatoare electrolitice miniatură, polarizate, cu terminale axiale”); use: in coupling and decoupling circuits, allowing high ripple currents, for professional equipment; the products are made to STAS 7675-73 and IEC 103 [2]. The series is marked „*”: a product under development („în curs de omologare”) [2].
Construction, as given in the 1978–1979 catalogue: anode: high-purity aluminium foil; cathode: the electrolyte; dielectric: aluminium oxide; terminals: axial tinned copper wire, welded connections; protection: aluminium tubes sealed with rubber stoppers, a plastic covering on request [2].
Technical data (1978–1979 catalogue): class type 1; temperature range −25…+75 °C; climatic category 25/070/21; rated capacitance 4.7…220 µF; capacitance tolerances −10…+100 %; −10…+50 % (special); rated voltage 6.3; 10; 16; 25; 40; 63 V DC; leakage current at 20 °C ≤ 0.006·Cn·Un (µF·V) + 4 µA for Cn·Un ≤ 1000 µF·V; ≤ 0.01·Cn·Un (µF·V) + 1 (printed „µF”) for Cn·Un ≥ 1000 µF·V; tan δ at 20 °C, 100 Hz ≤ 30 % (Un = 6.3 V), ≤ 25 % (Un = 10…40 V), ≤ 20 % (Un = 63 V); ripple current the maximum values at 40 °C and 50 Hz are given in the table; ripple current against temperature fig. 62 (1 up to 40 °C, falling to 0 at 70 °C); reliability λ ≤ 10⁻⁶/h [2].
The 1978–1979 catalogue’s table lists 18 rows, EP 52.48…EP 52.57 (7 codes); ordering code example „EP 52.48 — 22/16” [2].
Dimensions in mm (fig. 61), 1978–1979 catalogue: D + 0.5, L ± 0.5, R (between the bent leads) and A (lead length) from the table; leads Ø 0.8, 38–52 and 33–38 mm long [2]. The 1978–1979 catalogue also has fig. 62 („Variation of the ripple current with the temperature”); the drawings and graphs are under Drawing Gallery [2].
In the 1978–1979 catalogue, the class is „tip 1” (the EG 52.00 and ET 52.00: „tip 2”); the leakage-current limits are those the introduction gives for „long life” capacitors, but with the two conditions the other way round (the introduction: 0.01·Cn·Un or 1 µA for Cn·Un ≤ 1000, 0.006·Cn·Un + 4 µA above) [2].
The catalogue’s introduction to aluminium electrolytic capacitors (1978–1979) explains that they rest on the „valve” property of the oxide–metal structure, the oxide blocking the current in one direction and letting it pass in the other; they are wound: the anode is a high-purity aluminium foil on which a layer of aluminium oxide is formed anodically, the second armature is a conducting liquid (the electrolyte), and the aluminium foil called „cathode” only makes the contact with the electrolyte; the foils are separated by layers of paper that hold the electrolyte (fig. 51). The rated voltage Un is the DC voltage that can be applied between the minimum and maximum category temperatures, with the + pole on the anode (connected the other way, the capacitor is destroyed); the peak voltage Uv, allowed for at most a minute about 5 times an hour, is 1.15 Un for Un ≤ 100 V and 1.10 Un for Un > 100 V. With an AC voltage superimposed, the peak must not exceed Un and no reverse voltage above 1 V may appear (except on non-polarised capacitors). The ripple currents are r.m.s. values at 50 Hz and 40 °C; they fall with temperature (fig. 52, to zero at the maximum category temperature) and may be multiplied by 1.2 at 100 Hz, 1.4 at 500 Hz, 1.5 at 1000 Hz and 1.6 at 2000 Hz and above. The leakage current falls in 30–60 minutes to a constant value (fig. 53; curve b after a long storage without voltage), rises with temperature (fig. 54; factors 0.5 at 0 °C, 1 at 20 °C, 4 at 50 °C, 5 at 60 °C, 6 at 70 °C and 10 at 85 °C, and 0.8, 1, 1.5, 2 and 2.5 at 15, 20, 25, 30 and 35 °C) and with the voltage (fig. 55, up to the forming voltage UF); it is checked after 5 minutes at Un and 20 °C, the limits being 0.01·Cn·Un or 1 µA (the larger) for Cn·Un ≤ 1000 and 0.006·Cn·Un + 4 µA above for „long life” capacitors, and 0.05·Cn·Un or 5 µA, or 0.03·Cn·Un + 20 µA, for general-purpose ones (Cn in µF, Un in V), after a reconditioning: Un for one hour through 100 Ω (Un ≤ 100 V) or 1000 Ω (Un > 100 V), then 12–200 hours without voltage at 15–35 °C. The capacitance and tan δ are measured at 100 or 120 Hz, 0.5 V AC and 20 °C; the capacitance changes with temperature (fig. 56, more steeply for lower rated voltages), falls with frequency, especially at low temperatures, and drifts more in time at low rated voltages, high temperatures and large ripple currents; tan δ rises with frequency to a maximum that moves to higher frequencies as the temperature rises (fig. 57); the equivalent series resistance is ESR = tan δ/2πfC, and the impedance (fig. 58) follows the capacitive reactance at low frequencies, falls to about the ESR and rises again above the resonance. Stored without voltage, above all when hot, the electrolyte attacks the oxide layer: the capacitors can be kept at least a year without voltage, but the current in the first minutes after switching on may then be 100 times larger. They are marked in clear [3]. The introduction’s drawing and graphs for electrolytic capacitors (pp. 131–136: section of the winding, ripple current, leakage current, capacitance, tan δ and impedance, figs. 51–58) are under Drawing Gallery [3].
Drawing Gallery
No image available
No image available
No image available
No image available
No image available
No image available
No image available
No image available
No image available
No image availablePhoto Gallery
No other images available yet.
Documents
No documents available yet.
Prices
N/A
References
- [1]N. Millea, I. Constantinescu (coord.) – „Un secol de electronică în România”, Editura Academiei Române, 2020, section VIII.1.2.6, pp. 408–411
- [2]I.P.R.S. Băneasa – „Condensatoare / Capacitors”, catalogue 1978–1979 (published by ICCE), section „Electrolytic capacitors”, „Polarized miniature axial terminal electrolytic capacitors” EP 52.00, pp. 152–155
- [3]I.P.R.S. Băneasa – „Condensatoare / Capacitors”, catalogue 1978–1979 (published by ICCE), section „Electrolytic capacitors”, „Generalități – Principalii parametri de lucru”, pp. 131–136